[an error occurred while processing this directive]
 
       首 页  |  期刊介绍  |  编委会  |  投稿指南  |  期刊订阅  |  广告合作  |  留言板  |  联系我们 |  English
现代隧道技术 2022, Vol. 59 Issue (1) :256-262    DOI:
新型材料与设备 最新目录 | 下期目录 | 过刊浏览 | 高级检索 << [an error occurred while processing this directive] | [an error occurred while processing this directive] >>
海底隧道注浆材料耐腐蚀性能研究及工程应用
(中铁十五局集团城市轨道交通工程有限公司,洛阳 471002)
Study on Corrosion Resistance of Grouting Materials for Subsea Tunnels and Its Engineering Application
(Urban Rail Transit Engineering Company Limited of China Railway 15th Bureau, Luoyang 471002)
Download: PDF (2163KB)   HTML (1KB)   Export: BibTeX or EndNote (RIS)      Supporting Info
摘要 海水具有较强的腐蚀性,极容易通过围岩薄弱区域侵蚀破坏隧道衬砌结构,为保证支护结构的耐久性,文章以普通硅酸盐水泥为基材,通过调节减水剂、速凝剂和高分子聚合物的掺量来设计耐腐蚀注浆材料的配合比,并对不同配合比注浆材料进行了耐腐蚀指标测试和现场注浆效果检验。室内试验结果表明,该注浆材料试块(水灰比为0.65~1.0)在海水浸泡360 d的强度腐蚀系数大于0.80,体积稳定性良好;为加快侵蚀速度,将试块浸泡在饱和MgSO4溶液中,注浆材料试块(水灰比为0.65)浸泡360 d的强度腐蚀系数大于0.80,体积稳定性仍良好。通过现场注浆试验对结石体强度进行测试,测试结果表明,在饱和MgSO4溶液中浸泡180 d的浆液结石体的点荷载强度均值为0.931 kN,比未浸泡试块的强度均值0.984 kN减少了5.5%,进一步验证了注浆材料的耐腐蚀性能。
Service
把本文推荐给朋友
加入我的书架
加入引用管理器
Email Alert
RSS
作者相关文章
焦 雷
关键词海底隧道   注浆材料   耐腐蚀性   强度腐蚀系数   体积稳定性     
Abstract: Seawater is highly corrosive, and it is very easy to cause erosion and destruction of tunnel lining structure through the weak area of surrounding rocks. In order to ensure the durability of the supporting structure, the mix proportion of corrosion-resistant grouting materials with ordinary Portland cement as the base material is designed by means of adjusting the content of water reducer, accelerator and high molecular polymer, and the corrosion-resistant index test and field grouting effect test are carried out on grouting materials with different mix proportions. The indoor test results show that the strength corrosion coefficient of the grouting material sample (water-cement ratio:0.65~1.0) after 360 d soaking in seawater is greater than 0.80, with good volume stability. In order to accelerate the erosion rate, the test sample is soaked in saturated MgSO4 solution, and the strength corrosion coefficient of the grouting material sample (water-cement ratio: 0.65) after 360 d soaking is greater than 0.80, and still with good volume stability. The strength of set grouts is tested through field grouting test. The test results show that the average point load strength of set grouts after 180 d soaking in saturated MgSO4 solution is 0.931 kN, which is 5.5% lower than the average strength 0.984 kN of non-soaked samples, further verifying the corrosion resistance of grouting materials.
KeywordsSubsea tunnel,   Grouting materials,   Corrosion resistance,   Strength corrosion coefficient,   Volume stability     
收稿日期: 2021-03-05;
作者简介: 焦 雷(1985-),男,硕士,高级工程师,主要从事隧道与地下工程施工管理与科研工作,E-mail:270467094@qq.com.
引用本文:   
焦 雷 .海底隧道注浆材料耐腐蚀性能研究及工程应用[J]  现代隧道技术, 2022,V59(1): 256-262
JIAO Lei .Study on Corrosion Resistance of Grouting Materials for Subsea Tunnels and Its Engineering Application[J]  MODERN TUNNELLING TECHNOLOGY, 2022,V59(1): 256-262
链接本文:  
http://www.xdsdjs.com/CN/      或     http://www.xdsdjs.com/CN/Y2022/V59/I1/256
 
没有本文参考文献
[1] 董建松.厦门海沧海底隧道穿越风化槽施工技术[J]. 现代隧道技术, 2021,58(6): 197-203
[2] 高鹏鹏 1 徐 方 1 宋普涛 2 王宁宁 3 张 伟 4.高性能同步注浆材料对富水砂层盾构施工参数的影响研究[J]. 现代隧道技术, 2021,58(6): 244-250
[3] 杜宝义 1 宋超业 1 贺维国 1 李 凯 2.海底隧道钻爆法与盾构法交接技术及应用[J]. 现代隧道技术, 2021,58(2): 208-213
[4] 秦鹏飞.地下工程注浆技术研究新进展[J]. 现代隧道技术, 2020,57(2): 55-60
[5] 杨 钊 1,3 贺祖浩 1,2 刘 毅 1,2 陈培帅 1,2 李德杰 1,3.福州地铁过江通道泥水盾构弃浆在壁后注浆材料中的再利用[J]. 现代隧道技术, 2019,56(3): 192-199
[6] 吴金刚.妈湾通道前海湾海底隧道沉管法技术可行性研究[J]. 现代隧道技术, 2018,55(3): 28-36
[7] 宋超业, 贺维国.氯化物环境暗挖海底隧道支护结构的耐久性设计[J]. 现代隧道技术, 2016,53(2): 165-172
[8] 李永宽1,2 张顶立1 房 倩1.海底隧道建设全过程风险评估分析[J]. 现代隧道技术, 2015,52(3): 47-54
[9] 赵成龙1, 2, 李术才1, 徐帮树1, 张乐文1.动态增量位移正算反演分析及其在隧道工程中的应用[J]. 现代隧道技术, 2014,51(6): 78-82
[10] 朱朝佐.复杂机房风道互通群洞施工技术[J]. 现代隧道技术, 2014,51(2): 122-126
[11] 程选生1, 2 王建华1 杜修力2.渗流作用下海底隧道的流-固耦合地震响应分析[J]. 现代隧道技术, 2013,50(6): 44-51
[12] 谢文清 杨龙伟 吴登奎.胶州湾海底隧道快速超前帷幕注浆施工技术[J]. 现代隧道技术, 2013,50(3): 147-152
[13] 李沿宗 李治国 王全胜 焦雷.钻爆法海底隧道软弱破碎地层注浆加固堵水技术浅析[J]. 现代隧道技术, 2013,50(2): 26-33
Copyright 2010 by 现代隧道技术